Opalscent, Nihon Shippo Enamel for Copper, Silver, Gold, Iron and Steel. This enamel is "medium fusing" and should be fired at 1450 to 1550 degrees F. for approximately 2 to 4 minutes. The enamel is lead bearing |
|||||
| |||||
| |||||
|