- Listing of Enamels >
- W.G. Ball Enamel >
Wet Process/Dry Form For Steel
| | | |
|
|
High quality Wet Process Enamel in dry form for Steel To achieve our recommended thickness of enamel, put 8 parts by weight of wet process dry powder into a suitable sized container then add 3 parts by weight of boiling water and stir until smooth, leave it to cool down and it is then ready to use. If you prefer, you can vary the powder to water ratio to suit your requirements. Once a layer of sheet steel groundcoat has been applied to the steel and fired, all other wet process enamels and normal jewellery enamels can be used. The method of production of the fired trials was as follows:- The metal was degreased. Sheet steel groundcoat was applied by spraying. The enamels can also be dipped or the enamel applied with a soft brush. The enamel was dried and fired for 3 minutes at 1472F. One coat of wet process white was applied and fired at the same temperature, and then two coats of each colour were applied and fired to give a solid opaque colour. The actual size of the tile is 10cm c 10cm and the gauge of metal was 1.6mm This is a lead-free enamel
|
|
|